Burroughs' Encyclopaedia. The Process of Giving a Tempered-Blue Color to the Steel Plate and Malleable Iron Castings of a Roller Skate.

Burroughs' Encyclopaedia of Astounding Facts and Useful Information
Barkham Burroughs
1889
In order to obtain an even blue, the work must have an even finish, and be made perfectly clean. Arrange a cast-iron pot in a fire so as to heat it to the temperature of melted lead, or just below a red heat. Make a flat bottom basket of wire or wire cloth to sit in the iron box, on which place the work to be blued, as many pieces as you may find you can manage, always putting in pieces of about the same thickness and size, so that they will heat evenly. Make a bail to the basket, so that it can be easily handled. When the desired color is obtained, dip quickly in hot water to stop the progress of the bluing, for an instant only, so that enough heat may be retained to dry the articles. A cover to the iron box may sometimes be used to advantage to hasten the heating. Another way, much used, is to varnish the work with ultramarine varnish, which may be obtained from the varnish makers.

Ei kommentteja :